In the Hall -Heroult process, aluminium is formed at the cathode. The cathode is made out of :
Copper
Platinum
Carbon
Pure aluminium
Personalized AI Tutor and Adaptive Time Table, Self Study Material, Weekend Live Classes, Mentorship from our Experts, Unlimited Mock Tests and Personalized Analysis Reports, 24x7 Doubt Chat Support,.
Personalized AI Tutor and Adaptive Time Table, Self Study Material, Weekend Live Classes, Mentorship from our Experts, Unlimited Mock Tests and Personalized Analysis Reports, 24x7 Doubt Chat Support,.
Unlimited Chapter Wise Tests, Unlimited Subject Wise Tests, Unlimited Full Mock Tests, Get Personalized Performance Analysis Report,.
Personalized AI Tutor and Adaptive Time Table, Self Study Material, Weekend Live Classes, Mentorship from our Experts, Unlimited Mock Tests and Personalized Analysis Reports, 24x7 Doubt Chat Support,.
Booster and Kadha Video Lectures, Unlimited Full Mock Test, Adaptive Time Table, 24x7 Doubt Chat Support,.
Hall and Heroult Process -
Use to extract aluminum. A fuse mixture of alumina (20%), cryolite (60%) and fluorspar (20%) is electrolyzed using carbon electrodes.
- wherein
Cryolite makes Al2O3 conducting, fluorspar decreases the melting point of alumina
As we have learned that in the Hall -Heroult process,cathode is made up of caarbon
Option 1)
Copper
Option 2)Platinum
Option 3)Carbon
Option 4)Pure aluminium